冷轧辊常用材料有;9Cr,9Cr2,9Crv,8CrMov等,冷轧辊要求表面淬火,硬度HS45-105.热轧辊常用材料有;55Mn2,55Cr,60CrMnMo,60SiMnMo等,热轧辊要求整体正火或淬火,硬度HB190-270.